Wear resistant steels - data sheets
-
DILLIDUR 325 L - Air hardened wear resistant steel
July 2002, Size: 18 KBytes -
DILLIDUR 400 V - Water quenched wear resistant steel
March 2010, Size: 85 KBytes -
DILLIDUR 450 V - Water quenched wear resistant steel
March 2010, Size: 88 KBytes -
DILLIDUR 500 V - Water quenched wear resistant steel
March 2010, Size: 87 KBytes
Wear resistant steels - specifications
-
ABRACORR 30 - Wear resistant steel plate with enhanced corrosion resistance
December 2003, Size: 108 KBytes -
DILLIDUR IMPACT - Water quenched wear resistant steel
December 2010, Size: 203 KBytes
High strength steels - data sheets
-
DILLIMAX 500 - High strength fine grained structural steel, quenched and tempered
April 2003, Size: 25 KBytes -
DILLIMAX 550 - High strength fine grained structural steel, quenched and tempered
April 2003, Size: 133 KBytes -
DILLIMAX 690 - High strength fine grained structural steel, quenched and tempered
March 2010, Size: 135 KBytes -
DILLIMAX 890 - High strength fine grained structural steel, quenched and tempered
March 2010, Size: 135 KBytes -
DILLIMAX 965 - High strength fine grained structural steel, quenched and tempered
May 2011, Size: 171 KBytes
High strength steels - specifications
-
DILLIMAX 1100 - High strength fine grained structural steel, quenched and tempered
May 2011, Size: 170 KBytes -
DILLIMAX TL - High strength fine grained structural steels for telescopic crane booms
September 2010, Size: 112 KBytes -
DI-MC 550 - Weldable fine grained structural steel, thermomechanically rolled
September 1999, Size: 15 KBytes
Special specifications
-
DICUT - Heavy plates with improved laser properties
December 2011, Size: 147 KBytes -
OFL-L-LIFTARM- Plates with high surface quality for lift arms
December 2010, Size: 111 KBytes
Further information about feasibility and prices are available in our e-service-area: