Production
|
|
2007 |
2008 |
2009 |
2010 |
||
|---|---|---|---|---|---|---|
|
Crude steel production |
kt |
2,655 |
2,619 |
1,922 |
2,125 |
|
|
Heavy plate production in total |
kt |
2,388 |
2,227 |
1,609 |
1,882 |
|
|
at Dillingen |
kt |
1,607 |
1,481 |
1,147 |
1,216 |
|
|
at Dunkirk (GTS) |
kt |
781 |
746 |
462 |
666 |
Employees (without trainees)
|
|
2007 |
2008 |
2009 |
2010 |
||
|---|---|---|---|---|---|---|
|
at Dillingen |
per 31.12. |
5,233 |
5,322 |
5,296 |
5,412 |
|
|
at Dunkirk (GTS) |
per 31.12. |
618 |
626 |
611 |
590 |
Key financial data Dillinger Hütte
|
|
2007 |
2008 |
2009 |
2010 |
||
|---|---|---|---|---|---|---|
|
Sales |
Mio. € |
2,626 |
3,032 |
2,161 |
1,955 |
|
|
EBITDA |
Mio. € |
558 |
613 |
421 |
214 |
|
|
EBIT |
Mio. € |
493 |
549 |
361 |
158 |
Key financial data and total of employees of Dillinger Hütte Group (DHS consolidated)
|
|
2007 |
2008 |
2009 |
2010 |
||
|---|---|---|---|---|---|---|
|
Sales |
Mio. € |
2,898 |
3,305 |
2,258 |
2,110 |
|
|
EBITDA |
Mio. € |
811 |
960 |
232 |
458 |
|
|
EBIT |
Mio. € |
731 |
890 |
131 |
368 |
|
|
Employees |
per 31.12. |
8,278 |
8,494 |
8,178 |
8,072 |
-
Annual Report Dillinger Hütte (2010, only in German)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2010, Size: 1291 KBytes -
DHS consolidated financial statements (2010, only in German)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2010, Size: 692 KBytes -
Summarized English-language financial statement (2010) *
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2010, Size: 543 KBytes
* This summarized English-language financial statement is an excerpt from the annual report of Aktien-Gesellschaft der Dillinger Hüttenwerke for the 2010 financial year. This does not constitute a publication corresponding to the form required by law (for this, please see the 2010 Annual Report of Aktien-Gesellschaft der Dillinger Hüttenwerke in German).
-
Annual Report Dillinger Hütte (2009, only in German)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2009, Size: 3 MBytes -
DHS consolidated financial statements (2009, only in German)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2009, Size: 932 KBytes -
Summarized English-language financial statement (2009) *
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2009, Size: 2 MBytes
* This summarized English-language financial statement is an excerpt from the annual report of Aktien-Gesellschaft der Dillinger Hüttenwerke for the 2009 financial year. This does not constitute a publication corresponding to the form required by law (for this, please see the 2009 Annual Report of Aktien-Gesellschaft der Dillinger Hüttenwerke in German).
-
Annual Report Dillinger Hütte (2008, only in German)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2008, Size: 6 MBytes -
Summarized English-language financial statement (2008) *
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2008, Size: 2 MBytes
* This summarized English-language financial statement is an excerpt from the annual report of Aktien-Gesellschaft der Dillinger Hüttenwerke for the 2008 financial year. This does not constitute a publication corresponding to the form required by law (for this, please see the 2008 Annual Report of Aktien-Gesellschaft der Dillinger Hüttenwerke in German).
-
Annual Report Dillinger Hütte (2007, only in German)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2007, Size: 4 MBytes -
Summarized English-language financial statement (2007)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2007, Size: 2 MBytes
* This summarized English-language financial statement is an excerpt from the annual report of Aktien-Gesellschaft der Dillinger Hüttenwerke for the 2007 financial year. This does not constitute a publication corresponding to the form required by law (for this, please see the 2007 Annual Report of Aktien-Gesellschaft der Dillinger Hüttenwerke in German).
-
Annual Report Dillinger Hütte (2006, only in German)
Aktien-Gesellschaft der Dillinger Hüttenwerke, 2006, Size: 3 MBytes