06. December 2013
DILLIMAX 690 T is now available in thicknesses up to 250 mm from Dillinger Hütte group’s stocks. In October and November, the first heavy plates arrived in the stockyards of Ancofer Stahlhandel GmbH and AncoferWaldram Steelplates B.V. The DILLIMAX stock range is now extended to ultra thick plates.
During bauma 2013 in Munich, Dillinger Hütte GTS presented the new DILLIMAX 690. The maximum plate thickness is now 250 mm.
The carbon equivalents are restricted to significantly lower values than in EN standards. This allows for safe and economic welding. Low carbon equivalents stand for low preheat temperatures and consequently lower fabrication costs. Since April the first orders of this special grade have successfully been delivered. The extension of the DILLIMAX stock range up to 250 mm will help to serve quick needs of plates and oxy cut parts.
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz
Imprint
Data privacy statement
T&C