28. July 2017
On a safe track
Occasionally, also for offshore wind farms, construction material with a mark showing the conformity to the Construction Products Regulation (CPR) is demanded (CE-mark) either by rules or by the end customer. This means for heavy plates, that they have to comply with the harmonized standard EN 10025. However, because of the better toughness properties as well as the better weldability offshore steel grades according to EN 10225 are often requested by designers and fabricators (e.g. for substations, jackets etc.).
As EN 10225 is not a harmonized standard, it is insufficient for issuing a CE mark.
DIWIND offers you via a combination of two steel grades the down-to-earth solution: High offshore steel grades, as needed for your project, with CE marking. Additionally it guaranties even further improved carbon equivalents compared to the offshore standard EN 10225.
So, be on the safe track - from regulations as well as from a fabrication point of view.
Further information:
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz
Imprint
Data privacy statement
T&C