08. February 2016
Dillinger structural steel plates according to DBS 918002-02 now on stock at Ancofer
Due to increasing demand, Ancofer in Mülheim, Germany, now stocks Dillinger structural steel plates S355J2+N according to Deutsche Bahn (German Railways) guideline DBS 918002-02.
Dillinger Hütte, as HPQ-qualified supplier, certifies a so called weld-bend test for these plates thicker than 30 mm. Furthermore, 3.2-certificates are issued for all these stocked plates ranging up to 60 mm thickness and 2,500 mm width.
Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.
© 2016 Dillinger All rights reserved.
AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar
Tel.: +49 6831 47 0
Fax: +49 6831 47 2212