Prestigious conference „Pressure Vessels & Piping®“ with DILLINGER participation

07. September 2020

DILLINGER presented the latest findings from its development of alloyed, creep-resistant CrMo steels to an international specialist audience:

UTILISATION LIMITS OF 1¼CR½MO (SA387-11-2) STEEL IN HIGH PLATE THICKNESS
authors: Dr. Ingo Detemple, Dr. Bastian Philippi, Jörg Maffert

The total of more than 200 contributions dealt with topics such as regulations and standards, construction, materials, manufacture and testing.

Due to the corona pandemic, the conference took place in virtual form. It started on August 3rd and will last until the beginning of November. As usual, the specialist articles are offered in the form of a conference proceedings.

When submitting the presentations, the applicants had to undergo a critical evaluation by a specialist committee. Dillinger proposal was already given top marks.


Contact

 Philipp Ludwig
Philipp Ludwig

Sales Hydraulic engineering, Pressure vessel & Boiler construction, Shipbuilding incl. low temperature transport

Tel.: +49 6831 472472
Fax: +49 6831 47992685
E-Mail

Dillinger

Contact

 Jörg Maffert
Jörg Maffert

Marketing & Technical Support

Tel.: +49 6831 473612
Fax: +49 6831 473089
E-Mail

Dillinger

Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.

© 2016 Dillinger All rights reserved.

Contact

AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar

Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz

Imprint Data privacy statement T&C

news@dillinger

Our newsletter news@dillinger informs you about interesting news and developments at Dillinger – the company, it’s products, examples of steel applications, processing instructions, etc.

Newsletter subscription

Press Releases
  • Archive
Downloads
  • Publications
  • Images
Newsletter
Links