Transcending boundaries

27. April 2017

Dillinger supplies steel for arched bridges on the new tram line from Strasbourg to Kehl

After long years of planning, its official inaugural celebration will take place this coming weekend (29./30. April 2017): the extension of Tram Line D from Strasbourg in France to Kehl in Germany. Special steel from Dillinger will play an essential role here in transcending the boundary(ies).

This is because, in order to reach the river Rhine which marks the border, the tram route must cross the Vauban basin. This is achieved by travelling across the newly constructed Pont Citadelle, a 163 metre-long vaulted arch bridge with an arch that rises ornately 40 metres above the surface of the water. When it reaches the Rhine, the new tram crosses it via a 290 metre-long and 16 metre-wide double arched bridge with two arches, each 20 metres in height, until it arrives on the banks at Kehl. Like the Citadelle bridge, the tram bridge across the Rhine also offers space for pedestrians and cyclists.

For these two unique bridge structures, Dillinger supplied a total of around 3,500 tonnes of mainly higher-strength, thermomechanically rolled steel with plate thicknesses of up to 115 millimetres – and is thus playing a part in ensuring that the tram can henceforth travel from what is presently the end of the line at Aristide Briand to the station at Kehl.

 

©Dillinger

©Dillinger

©Dillinger ©Dillinger

Contact

 Ute Engel
Ute Engel

Head of Public relations

Tel.: +49 6898 102265
Fax: +49 6898 104014
E-Mail

Dillinger

Contact

 Juliane Wernet
Juliane Wernet

Public relations

Tel.: +49 6898 102234
Fax: +49 6898 104014
E-Mail

Dillinger

Contact

 Martin Reinicke
Martin Reinicke

Public relations

Tel.: +49 6898 102211
Fax: +49 6898 104014
E-Mail

Dillinger

Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.

© 2016 Dillinger All rights reserved.

Contact

AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar

Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz

Imprint Data privacy statement T&C

news@dillinger

Our newsletter news@dillinger informs you about interesting news and developments at Dillinger – the company, it’s products, examples of steel applications, processing instructions, etc.

Newsletter subscription

Press Releases
  • Archive
Downloads
  • Publications
  • Images
Newsletter
Links