  • Heavy-plate products
    • Non-alloy structural steels
    • Normalised fine-grained structural steels
    • Thermomechanically rolled fine-grained steels
    • High-strength quenched & tempered fine-grained steels
    • High-temperature steels
    • Cryogenic steels
    • Weathering-resistant steels
    • Case-hardening & quenching & tempering steels
    • Security steels
    • Tool & mould steels
    • Wear-resistant steels
    • Sour-gas-resistant steels
    • Offshore steels
    • Linepipe steels
  • Applications
    • Steel Construction
    • Hydropower Engineering
    • Pressure Vessels & Boilers
    • Earthmoving Machinery & Mining
    • Mechanical Engineering
    • Offshore Oil & Gas
    • Large Diameter Pipes
    • Shipbuilding, inc. Refrigerated Transport
    • Plastics and Concrete Moulds
    • Wind & Tidal Power
    • Protection
  • Proprietary steels
    • DILLIDUR
    • DILLIMAX
    • DI-MC
    • DIWETEN
    • DICREST
    • DIWA
    • DILLINAL
    • DIROS
    • DIMO
    • DIFENDER
    • DICUT
    • DI-RACK
    • DIGEAR
    • DI-TANK
    • DIWIND
    • Other steels
  • Plates on stock and steel services
    • Heavy plate services ex stock
    • Heavy plate services ex mill
    • Components ex stock
  • By-products & Chemical laboratrory
    • By-products
    • Chemical laboratrory services
Banner
  1. Products
  2. Heavy-plate products
  3. Wear-resistant steels

Wear-resistant steels

Standing up to wear for long service-lives

Dillinger's wear-resistant steels assure extreme resistance to abrasive wear, and thus significantly lengthen the service-life of components exposed to extreme wear in vehicles, industrial plants, machinery, handling and conveying systems and attachments in earthmoving, highway construction, recycling and mining, quarries, cement plants and steel mills, for example.

 

The Dillinger range for your needs:

  • Dillinger supplies a broad range of diverse grades and size formats, in thicknesses extending from 8 mm to around 200 mm.
  • Our DILLIDUR proprietary steel is the result of more than 50 years of experience and unceasing further development, conducted in cooperation with renowned original-equipment suppliers.
  • These steels incorporate a balanced alloying concept and possess pleasant working and welding properties.
  • Low preheat temperatures prior to welding and flame-cutting assure greater safety margins during workshop fabrication and on-site repairs under adverse conditions.

Applications

Earthmoving Machinery & Mining

Mechanical Engineering

Proprietary steels

DILLIDUR

DIGEAR

Feasibility

Product finder and feasibility check (E-Service)

Contact

 Christoph Dickmann
Christoph Dickmann

Sales Earth moving & Mining equipment, Heavy Machinery, Mold & Die construction

Tel.: +49 6831 472385
Fax: +49 6831 47992681
E-Mail

Dillinger

Contact

Dr. Wolfram Hölbling
Dr. Wolfram Hölbling

General Manager Marketing & Technical Support

Tel.: +49 6831 474708
Fax: +49 6831 473089
E-Mail

Dillinger

Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.

© 2016 Dillinger All rights reserved.

Contact

AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar

Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz

Imprint Data privacy statement T&C

news@dillinger

Our newsletter news@dillinger informs you about interesting news and developments at Dillinger – the company, it’s products, examples of steel applications, processing instructions, etc.

Newsletter subscription

Heavy-plate products
  • Non-alloy structural steels
  • Normalised fine-grained structural steels
  • Thermomechanically rolled fine-grained steels
  • High-strength quenched & tempered fine-grained steels
  • High-temperature steels
  • Cryogenic steels
  • Weathering-resistant steels
  • Case-hardening & quenching & tempering steels
  • Security steels
  • Tool & mould steels
  • Wear-resistant steels
  • Sour-gas-resistant steels
  • Offshore steels
  • Linepipe steels
Applications
  • Steel Construction
  • Hydropower Engineering
  • Pressure Vessels & Boilers
  • Earthmoving Machinery & Mining
  • Mechanical Engineering
  • Offshore Oil & Gas
  • Large Diameter Pipes
  • Shipbuilding, inc. Refrigerated Transport
  • Plastics and Concrete Moulds
  • Wind & Tidal Power
  • Protection
Proprietary steels
  • DILLIDUR
  • DILLIMAX
  • DI-MC
  • DIWETEN
  • DICREST
  • DIWA
  • DILLINAL
  • DIROS
  • DIMO
  • DIFENDER
  • DICUT
  • DI-RACK
  • DIGEAR
  • DI-TANK
  • DIWIND
  • Other steels
Plates on stock and steel services
  • Heavy plate services ex stock
  • Heavy plate services ex mill
  • Components ex stock
By-products & Chemical laboratrory
  • By-products
  • Chemical laboratrory services