  • Heavy-plate products
    • Non-alloy structural steels
    • Normalised fine-grained structural steels
    • Thermomechanically rolled fine-grained steels
    • High-strength quenched & tempered fine-grained steels
    • High-temperature steels
    • Cryogenic steels
    • Weathering-resistant steels
    • Case-hardening & quenching & tempering steels
    • Security steels
    • Tool & mould steels
    • Wear-resistant steels
    • Sour-gas-resistant steels
    • Offshore steels
    • Linepipe steels
  • Applications
    • Steel Construction
    • Hydropower Engineering
    • Pressure Vessels
    • Earthmoving Machinery & Mining
    • Mechanical Engineering
    • Offshore Oil & Gas
    • Large Diameter Pipes
    • Shipbuilding & Jackup
    • Plastics and Concrete Moulds
    • Wind Power
    • Protection
    • Steel & Service Center and Plate Processing
  • Proprietary steels
    • DILLIDUR
    • DILLIMAX
    • DI-MC
    • DIWETEN
    • DICREST
    • DIWA
    • DILLINAL
    • DIROS
    • DIMO
    • DIFENDER
    • DICUT
    • DI-RACK
    • DIGEAR
    • DI-TANK
    • DIWIND
    • Other steels
  • Plates on stock and steel services
    • Heavy plate services ex stock
    • Heavy plate services ex mill
  • By-products & Chemical laboratrory
    • By-products
    • Chemical laboratrory services
Banner
  1. Products
  2. Proprietary steels
  3. DILLIMAX

DILLIMAX

For ultra-high loads in earthmoving machines, offshore and structural steel

Ultra-high mechanical strength, but nonetheless extremely tough and exceptionally easy to work and weld – these properties make DILLIMAX the ideal solution for slender machine designs and load-bearing structures for the heaviest loads, where high precision and uncompromising safety are needed.

 

The strengths of DILLIMAX:

  • DILLIMAX is available in a large number of different variants – up to minimum yield strengths of 1,100 MPa, in plate thicknesses of up to 290 mm, and also in the form of Grade E to meet extreme toughness requirements at temperatures of -60 °C.
  • We guarantee for the widely used DILLIMAX 690T grade significantly higher Charpy V-notch toughnesses than specified in the EN 10025, Part 6, and ASTM A514 standards, assuring you of additional safety against cracking during processing and use than in the case of standard grades.
  • You benefit from the high cleanness and homogeneity of all DILLIMAX steels, with an in-works UT ultrasonic guarantee over and above the applicable standard (S1 E1 in accordance with EN 10160) and extremely low limits for phosphorus and sulphur contents.
  • Despite these steels' high mechanical strength, their low carbon equivalents permit sure and cost-effective welding.
  • Customers can, if they wish, also agree with us strict ultrasonic-inspection requirements and guaranteed properties in the plate-thickness direction (Z grade in accordance with EN 10164) for extremely thick plates.
  • DILLIMAX can also be ordered to DIPLAN specifications to assure excellent flatness across the entire steel surface. DILLIMAX TL assures ultra-tight thickness tolerances for crane booms.
  • Thanks to its exceptionally homogenous internal properties in even extremely thick plates, DILLIMAX is approved in accordance with DNV and ABS standards, for example, for particularly sensitive offshore applications.

 

Heavy-plate products

High-strength quenched and tempered fine-grained structural steels

Applications

Steel Construction

Hydropower Engineering

Earthmoving Machinery & Mining

Offshore Oil & Gas

Further information

Customer information

Data sheets & specifications

Processing instructions

DILLIMAX steels ex stock

First choice specialists keep our DILLIMAX steels in stock for you worldwide.

DILLIMAX steels ex stock

Feasibility

Product finder and feasibility check (E-Service)

Contact

 Christoph Dickmann
Christoph Dickmann

Head of Sales Department, Machinery & Construction Equipment, Protection

Tel.: +49 6831 472385
Fax: +49 6831 47992681
E-Mail

Dillinger

Contact

 Johannes Klemm
Johannes Klemm

Head of Marketing & Technical Support Department Machinery & Construction Equipment, Steel Service Center, Plate Processing

Tel.: +49 6831 475658
Fax: +49 6831 47999036
E-Mail

Dillinger

Innovative top-quality steel products, total orientation around our customers' needs and unceasing technological development in close cooperation with our partners form the basis of our success - as they have for more than 333 years.

© 2016 Dillinger All rights reserved.

Contact

AG der Dillinger Hüttenwerke
Werkstraße 1
66763 Dillingen/Saar

Tel.: +49 6831 47 0
Fax: +49 6831 47 2212
E-Mail: info@dillinger.biz

Imprint Data privacy statement T&C

news@dillinger

Our newsletter news@dillinger informs you about interesting news and developments at Dillinger – the company, it’s products, examples of steel applications, processing instructions, etc.

Newsletter subscription

Heavy-plate products
  • Non-alloy structural steels
  • Normalised fine-grained structural steels
  • Thermomechanically rolled fine-grained steels
  • High-strength quenched & tempered fine-grained steels
  • High-temperature steels
  • Cryogenic steels
  • Weathering-resistant steels
  • Case-hardening & quenching & tempering steels
  • Security steels
  • Tool & mould steels
  • Wear-resistant steels
  • Sour-gas-resistant steels
  • Offshore steels
  • Linepipe steels
Applications
  • Steel Construction
  • Hydropower Engineering
  • Pressure Vessels
  • Earthmoving Machinery & Mining
  • Mechanical Engineering
  • Offshore Oil & Gas
  • Large Diameter Pipes
  • Shipbuilding & Jackup
  • Plastics and Concrete Moulds
  • Wind Power
  • Protection
  • Steel & Service Center and Plate Processing
Proprietary steels
  • DILLIDUR
  • DILLIMAX
  • DI-MC
  • DIWETEN
  • DICREST
  • DIWA
  • DILLINAL
  • DIROS
  • DIMO
  • DIFENDER
  • DICUT
  • DI-RACK
  • DIGEAR
  • DI-TANK
  • DIWIND
  • Other steels
Plates on stock and steel services
  • Heavy plate services ex stock
  • Heavy plate services ex mill
By-products & Chemical laboratrory
  • By-products
  • Chemical laboratrory services